摘要: 通过平板撞击实验对铝锂合金层裂现象进行实验研究。以细观统计和唯象分析相结合的思想,提出了一种新的微孔洞型损伤演化方程,方程同时计及了孔洞长大、成核以及材料可压缩性的耦合效应对损伤演化的影响。在一维应变波模拟程序中嵌入考虑损伤演化影响的铝锂合金本构方程和状态方程,模拟平板撞击过程靶板自由面质点速度时程曲线,并与实验曲线相对比,得到了铝锂合金材料损伤演化方程及其层裂准则的相关参数。Abstract: The spallation experiments of Al-Li alloy have been carried out and the free surface velocity temporal curves for the spallation events have been measured. Based on the microscopics statistics and phenomenological analysis, a damage evolution equation is developed, which involves the effects of the growth and nucleation of microcavities as well as the effects of the material's compressibility. Inserting the constitutive equation and Murnagham state equation of Al-Li alloy and the damage evolution equation into ANWP, which is a special program for one-dimension strain wave, and by the numerical simulation of the free-surface velocity temporal curve for the spallation events in the gas gun experiments, we have obtained the related parameters in the damage evolution equation and the spallation criterion.
-
Key words:
- Al-Li alloy /
- damage evolution equation /
- spallation criterion /
- numerical simulation
-
Guo Y, Li Y C, Yao L, et al. Study on the Limit Strain-Rate Softening Property of Al-Li Alloy [J]. Explosion and Shock Waves, 2004, 24(1): 54-58. (in Chinese) 郭扬, 李永池, 姚磊, 等. 铝锂合金材料的极限应变率软化特性研究 [J]. 爆炸与冲击, 2004, 24(1): 54-58. Li Y C, Guo Y, Tan F L, et al. Equation of State for Al-Li Alloy [J]. Chinese Journal of High Pressure Physics, 2003, 17(2): 81-87. (in Chinese) 李永池, 郭扬, 谭福利, 等. 铝锂合金材料状态方程的研究 [J]. 高压物理学报, 2003, 17(2): 81-87. Seaman L, Curran D R, Shockey D A. Computational Models for Ductile and Brittle Fracture [J]. J Appl Phys, 1976, 47(11): 4814-4826. Perzyna P. Internal State Variable Description of Dynamic Fracture of Ductile Solids [J]. Int J Solids Struct, 1986, 22: 797-818. Feng J P. Damage Function Models for the Dynamic Ductile Fracture of Metals [D]. Beijing: Beijing Science and Technology University, 1992. (in Chinese) 封加波. 金属动态延性破坏的损伤度函数模型 [D]. 北京: 北京理工大学, 1992. Li Y C, Li D H, Wei Z G, et al. Research on the Deformation, Damage and Fracture Rules of Circular Tubes under Inside-Explosive Loading [J]. Acta Mechanica Sinica, 1999, 31(4): 442-449. (in Chinese) 李永池, 李大红, 魏志刚, 等. 内爆炸载荷下圆管变形、损伤和破坏规律的研究 [J]. 力学学报, 1999, 31(4): 442-449. Zhang L, Cai L C, Wang W, et al. The Response Feature for Shock Loading of Tantalum [J]. Chinese Journal of High Pressure Physics, 2001, 18(4): 255-270. (in Chinese). 张林, 蔡灵仓, 王悟, 等. 钽在冲击载荷下的动态力学特性 [J]. 高压物理学报, 2001, 18(4): 255-270.
点击查看大图
计量
- 文章访问数: 7833
- HTML全文浏览量: 330
- PDF下载量: 816