内爆加载下热塑性管壳的应力波演化与层裂效应研究

孙宇新 张进 李永池 胡时胜 董杰

孙宇新, 张进, 李永池, 胡时胜, 董杰. 内爆加载下热塑性管壳的应力波演化与层裂效应研究[J]. 高压物理学报, 2005, 19(4): 319-324 . doi: 10.11858/gywlxb.2005.04.006
引用本文: 孙宇新, 张进, 李永池, 胡时胜, 董杰. 内爆加载下热塑性管壳的应力波演化与层裂效应研究[J]. 高压物理学报, 2005, 19(4): 319-324 . doi: 10.11858/gywlxb.2005.04.006
SUN Yu-Xin, ZHANG Jin, LI Yong-Chi, HU Shi-Sheng, DONG Jie. Propagation of Stress wave and Spallation of Cylindrical Tube under External Explosive Loading[J]. Chinese Journal of High Pressure Physics, 2005, 19(4): 319-324 . doi: 10.11858/gywlxb.2005.04.006
Citation: SUN Yu-Xin, ZHANG Jin, LI Yong-Chi, HU Shi-Sheng, DONG Jie. Propagation of Stress wave and Spallation of Cylindrical Tube under External Explosive Loading[J]. Chinese Journal of High Pressure Physics, 2005, 19(4): 319-324 . doi: 10.11858/gywlxb.2005.04.006

内爆加载下热塑性管壳的应力波演化与层裂效应研究

doi: 10.11858/gywlxb.2005.04.006
详细信息
    通讯作者:

    孙宇新

Propagation of Stress wave and Spallation of Cylindrical Tube under External Explosive Loading

More Information
    Corresponding author: SUN Yu-Xin
  • 摘要: 在引入材料损伤软化、温度软化效应的基础上,对一维柱对称内聚爆加载管壳中应力波的传播、材料的变形和层裂问题开展了研究。成功地通过自编写有限元代码,完成了系列数值模拟计算,得到了管壁中与物理事实一致的应力波传播图像和材料的变形、损伤、层裂的发展规律,成功模拟了内聚爆加载管壳的多次层裂现象。

     

  • Nesterenko V F, Meyers M A, Wright T W. Shear Localization and Recrystallization in High-Strain, High-Strain-Rate Deformation of Tantalum [J]. Materials Science Engineering A: Structural Materials: Properties, Microstructure and Processing, 1997, A229: 23-41.
    Meyers M A, Nesterenko V F. High-Strain, High-Strain-Rate Deformation of Tantalum [J]. Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 1995, 26A: 2493-2501.
    Tang T G, Hu H B, Wang D S, et al. Shear Fracture of HR-2 Steel Tube under Shock Loading [J]. Chinese Journal of High Pressure Physics, 2002, 16(1): 75-79. (in Chinese)
    汤铁钢, 胡海波, 王德生, 等. 内爆压缩加载下抗氢钢圆管剪切断裂研究 [J]. 高压物理学报, 2002, 16(1): 75-79.
    Li X M. An Investigation on the Deformation, Damage and Spall of Cylindrical Steel Tube Loaded by Sliding-Implosion [D]. Hefei: University of Science and Technology of China, 2003. (in Chinese)
    李雪梅. 内爆加载下钢圆管的变形、损伤及层裂研究 [D]. 合肥: 中国科学技术大学, 2003.
    Li Y C, Li D H, Wei Z G, et al. Research on the Deformation, Damage and Fracture Rules of Circular Tubes under Inside-Explosive Loading [J]. Acta Mechanica Sinica, 1999, 31(4): 442-449. (in Chinese)
    李永池, 李大红, 魏志刚, 等. 内爆炸载荷下圆管变形、损伤和破坏规律的研究 [J]. 力学学报, 1999, 31(4): 442-449.